Remoção de corantes de efluente textil por zeólita de cinzas de carvão modificada por surfactante e avaliação dos efeitos tóxicos

Detalhes bibliográficos
Ano de defesa: 2015
Autor(a) principal: Patricia Cunico Ferreira
Orientador(a): Denise Alves Fungaro
Banca de defesa: Iara Maria Carneiro de Camargo, Juliana de Carvalho Izidoro, Deovaldo de Moraes Júnior, Camilo Dias Seabra Pereira
Tipo de documento: Tese
Tipo de acesso: Acesso aberto
Idioma: por
Instituição de defesa: Universidade de São Paulo
Programa de Pós-Graduação: Tecnologia Nuclear
Departamento: Não Informado pela instituição
País: BR
Link de acesso: https://doi.org/10.11606/T.85.2015.tde-17112015-095220
Resumo: Zeólitas sintetizadas a partir de cinzas leves e pesadas de carvão e modificadas com hexadeciltrimetilamônio (HDTMA) foram usadas como adsorvente para remoção dos corantes Solophenyl Navy (SN) e Solophenyl Turquesa (ST) e suas formas hidrolisadas, Solophenyl Navy hidrolisada (SNH) e Solophenyl Turquesa hidrolisada (STH), de efluente simulado de indústria têxtil. As zeólitas leve modificada (ZLM) e pesada modificada (ZPM) foram caracterizadas por diferentes técnicas, tais como, espectrometria de fluorescência de raios-X, difração de raios-X e microscopia eletrônica de varredura. As ZLM e ZPM apresentaram carga estrutural negativa devido à formação de uma bicamada parcial de HDTMA na superfície externa da zeólita. A concentração inicial dos corantes, o tempo de contato e o equilíbrio de adsorção foram avaliados. A cinética de adsorção de SN, ST, SNH e STH sobre as zeólitas seguiu o modelo de pseudo segunda- ordem. O tempo de equilíbrio foi de 20 min para SN e ST e 30 min para SNH e STH sobre ZLM, enquanto sobre ZPM foi de 60 min para SN e ST e 20 e 30 min para SNH e STH, respectivamente. Os modelos de Langmuir, Freundlich e Temkin foram aplicados para descrever as isotermas de adsorção. A adsorção dos corantes foi melhor descrita pelo modelo de Langmuir, com exceção dos sistemas SN/ZPM, SNH/ZPM e SNH/ZLM que seguiram modelo de Freundlich. As capacidades máximas de adsorção foram 3,64; 3,57; 2,91 e 4,93 mgL-1 para SN, ST, SNH e STH pela ZLM, respectivamente e 0,235; 0,492; 1,26 e 1,86 mgL-1 pela ZPM, nesta mesma ordem. O melhor desempenho dos corantes hidrolisados foi atribuído à redução do tamanho das moléculas dos corantes durante o processo de hidrólise. A toxicidade aguda dos corantes foi avaliada por diferentes organismos teste. O microcrustáceo C. dubia apresentou valores de EC50 de 1,25; 54,5; 0,78 e 2,56 mgL-1 para SN, ST, SNH e STH, respectivamente. A macrófita L. minor mostrou valores de EC50 de 18,9; 69,4; 10,9 e 70,9 mgL-1 para SN, ST, SNH e STH, respectivamente. As larvas de mosquitos C. tepperi mostraram valores de EC50 de 119 e 440 mgL-1 para a SN e ST, respectivamente. Com relação ao processo de adsorção, os efeitos agudos foram substancialmente reduzidos após o tratamento da solução aquosa de SN e ST com ZLM, assim como de suas formas hidrolisadas, apresentando nenhuma toxicidade após a remoção de 100% da cor. Após o tratamento dos corantes com ZPM houve um aumento da toxicidade, com exceção dos corantes SNH e STH que não apresentaram toxicidade após o tratamento. Testes de Avaliação e Identificação da Toxicidade foram realizados a fim de identificar quais substâncias estariam causando a toxicidade nos corantes SN, ST e no lixiviado de ZLM e ZPM. Os efeitos tóxicos foram reduzidos significativamente após a manipulação com Extração de Fase Sólida (SPE) e ácido etilenodiaminotetracético (EDTA) para o lixiviado de ZLM e ZPM. Os corantes mostraram redução na toxicidade após a manipulação com EDTA indicando que as substâncias tóxicas eram principalmente metais catiônicos.
id USP_fe0b16a8d30e989a2d230dcd6ef6efa0
oai_identifier_str oai:teses.usp.br:tde-17112015-095220
network_acronym_str USP
network_name_str Biblioteca Digital de Teses e Dissertações da USP
repository_id_str
spelling info:eu-repo/semantics/publishedVersioninfo:eu-repo/semantics/doctoralThesis Remoção de corantes de efluente textil por zeólita de cinzas de carvão modificada por surfactante e avaliação dos efeitos tóxicos Dyes removal of textile wastewater onto surfactant modified zeolite from coal ash and evaluation of the toxic effects 2015-09-15Denise Alves FungaroIara Maria Carneiro de CamargoJuliana de Carvalho IzidoroDeovaldo de Moraes JúniorCamilo Dias Seabra PereiraPatricia Cunico FerreiraUniversidade de São PauloTecnologia NuclearUSPBR adsorção adsorption carbon ash cinza de carvão corante direto corantes direct dyes dyes zeólita modificada por surfactante zeolite modified from surfactant Zeólitas sintetizadas a partir de cinzas leves e pesadas de carvão e modificadas com hexadeciltrimetilamônio (HDTMA) foram usadas como adsorvente para remoção dos corantes Solophenyl Navy (SN) e Solophenyl Turquesa (ST) e suas formas hidrolisadas, Solophenyl Navy hidrolisada (SNH) e Solophenyl Turquesa hidrolisada (STH), de efluente simulado de indústria têxtil. As zeólitas leve modificada (ZLM) e pesada modificada (ZPM) foram caracterizadas por diferentes técnicas, tais como, espectrometria de fluorescência de raios-X, difração de raios-X e microscopia eletrônica de varredura. As ZLM e ZPM apresentaram carga estrutural negativa devido à formação de uma bicamada parcial de HDTMA na superfície externa da zeólita. A concentração inicial dos corantes, o tempo de contato e o equilíbrio de adsorção foram avaliados. A cinética de adsorção de SN, ST, SNH e STH sobre as zeólitas seguiu o modelo de pseudo segunda- ordem. O tempo de equilíbrio foi de 20 min para SN e ST e 30 min para SNH e STH sobre ZLM, enquanto sobre ZPM foi de 60 min para SN e ST e 20 e 30 min para SNH e STH, respectivamente. Os modelos de Langmuir, Freundlich e Temkin foram aplicados para descrever as isotermas de adsorção. A adsorção dos corantes foi melhor descrita pelo modelo de Langmuir, com exceção dos sistemas SN/ZPM, SNH/ZPM e SNH/ZLM que seguiram modelo de Freundlich. As capacidades máximas de adsorção foram 3,64; 3,57; 2,91 e 4,93 mgL-1 para SN, ST, SNH e STH pela ZLM, respectivamente e 0,235; 0,492; 1,26 e 1,86 mgL-1 pela ZPM, nesta mesma ordem. O melhor desempenho dos corantes hidrolisados foi atribuído à redução do tamanho das moléculas dos corantes durante o processo de hidrólise. A toxicidade aguda dos corantes foi avaliada por diferentes organismos teste. O microcrustáceo C. dubia apresentou valores de EC50 de 1,25; 54,5; 0,78 e 2,56 mgL-1 para SN, ST, SNH e STH, respectivamente. A macrófita L. minor mostrou valores de EC50 de 18,9; 69,4; 10,9 e 70,9 mgL-1 para SN, ST, SNH e STH, respectivamente. As larvas de mosquitos C. tepperi mostraram valores de EC50 de 119 e 440 mgL-1 para a SN e ST, respectivamente. Com relação ao processo de adsorção, os efeitos agudos foram substancialmente reduzidos após o tratamento da solução aquosa de SN e ST com ZLM, assim como de suas formas hidrolisadas, apresentando nenhuma toxicidade após a remoção de 100% da cor. Após o tratamento dos corantes com ZPM houve um aumento da toxicidade, com exceção dos corantes SNH e STH que não apresentaram toxicidade após o tratamento. Testes de Avaliação e Identificação da Toxicidade foram realizados a fim de identificar quais substâncias estariam causando a toxicidade nos corantes SN, ST e no lixiviado de ZLM e ZPM. Os efeitos tóxicos foram reduzidos significativamente após a manipulação com Extração de Fase Sólida (SPE) e ácido etilenodiaminotetracético (EDTA) para o lixiviado de ZLM e ZPM. Os corantes mostraram redução na toxicidade após a manipulação com EDTA indicando que as substâncias tóxicas eram principalmente metais catiônicos. Zeolites synthesized from fly and bottom ashes and modified with hexadecyltrimethylamonium (HDTMA) were used as adsorbent to remove dyes - Solophenyl Navy (SN) and Solophenyl Turquoise (ST) and their hydrolysed forms Solophenyl Navy Hydrolysed (SNH) and Solophenyl Turquoise Hydrolysed (STH), from simulated textile wastewater. The HDTMA-modified fly zeolite (ZMF) and HDTMA-modified bottom zeolite (ZMB) were characterized by different techniques, as X-ray fluorescence spectrometry, X-ray diffraction and scanning electron microscopy, etc. The ZMF and ZMB presented negative charge probably due to the formation of a partial bilayer of HDTMA on exchangeable active sites on the external surface of unmodified zeolite. Initial dye concentration, contact time and equilibrium adsorption were evaluated. The adsorption kinetic for SN, ST, SNH and STH onto the zeolites followed the pseudo second-order model. The equilibrium time was 20 min for SN and ST and 30 min for SNH and STH, respectively. Langmuir, Freundlich and Temkin models were applied to describe the adsorption isotherms. Adsorption of the dyes were best described by the Langmuir model, with exception to SN/ZPM, SNH/ZPM and SNH/ZLM systems that followed Freundlich model. The maximum adsorption capacities were 3,64; 3,57; 2,91 e 4,93 for SN, ST, SNH e STH by ZLM, respectively and 0,235; 0,492; 1,26 e 1,86 by ZPM, in this order. The best performance for hydrolyzed dyes has been attributed to reduction of the size of dyes molecules during the hydrolysis process. Acute toxicity of the dyes to a different organism were evaluated by different test-organisms. Waterflea, Ceriodaphnia dubia showed EC50 value of 1,25; 54,5; 0,78 and 2,56 mgL-1 for SN, ST, SNH and STH, respectively. The plant Lemna minor showed EC50 values of 18,9; 69,4; 10,9 and 70,9 mgL-1 for SN, ST, SNH and STH, respectively. Midges larvae of Chironomus tepperi showed EC50 values of 119 and 440 mgL-1 for SN and ST, respectively. Regarding the adsorption process, acute effects were substantially reduced after adsorption treatment of aqueous solution with SN and ST by ZMF, as well as their hydrolysed forms, showing no toxicity after removal of 100% of colour. After treatment with ZPM there was an increase of the toxicity, with exception of SHN and STH dyes that do not show toxicity after the treatment. Toxicity Identification Evaluation tests (TIE) were realized in order to identify what substances were causing the observed toxicity for the SN, ST and the leached of ZMF and ZMB. The acute effects were significantly reduced after manipulation with Solid-Phase Extraction (SPE) and Ethylenediaminetetraacetic acid (EDTA) for the leached of ZMB and ZMF. The dyes showed reduced in the toxicity after manipulation with EDTA indicating that the toxicants are mostly cationic metals. https://doi.org/10.11606/T.85.2015.tde-17112015-095220info:eu-repo/semantics/openAccessporreponame:Biblioteca Digital de Teses e Dissertações da USPinstname:Universidade de São Paulo (USP)instacron:USP2023-12-21T19:15:10Zoai:teses.usp.br:tde-17112015-095220Biblioteca Digital de Teses e Dissertaçõeshttp://www.teses.usp.br/PUBhttp://www.teses.usp.br/cgi-bin/mtd2br.plvirginia@if.usp.br|| atendimento@aguia.usp.br||virginia@if.usp.bropendoar:27212016-07-28T16:11:58Biblioteca Digital de Teses e Dissertações da USP - Universidade de São Paulo (USP)false
dc.title.pt.fl_str_mv Remoção de corantes de efluente textil por zeólita de cinzas de carvão modificada por surfactante e avaliação dos efeitos tóxicos
dc.title.alternative.en.fl_str_mv Dyes removal of textile wastewater onto surfactant modified zeolite from coal ash and evaluation of the toxic effects
title Remoção de corantes de efluente textil por zeólita de cinzas de carvão modificada por surfactante e avaliação dos efeitos tóxicos
spellingShingle Remoção de corantes de efluente textil por zeólita de cinzas de carvão modificada por surfactante e avaliação dos efeitos tóxicos
Patricia Cunico Ferreira
title_short Remoção de corantes de efluente textil por zeólita de cinzas de carvão modificada por surfactante e avaliação dos efeitos tóxicos
title_full Remoção de corantes de efluente textil por zeólita de cinzas de carvão modificada por surfactante e avaliação dos efeitos tóxicos
title_fullStr Remoção de corantes de efluente textil por zeólita de cinzas de carvão modificada por surfactante e avaliação dos efeitos tóxicos
title_full_unstemmed Remoção de corantes de efluente textil por zeólita de cinzas de carvão modificada por surfactante e avaliação dos efeitos tóxicos
title_sort Remoção de corantes de efluente textil por zeólita de cinzas de carvão modificada por surfactante e avaliação dos efeitos tóxicos
author Patricia Cunico Ferreira
author_facet Patricia Cunico Ferreira
author_role author
dc.contributor.advisor1.fl_str_mv Denise Alves Fungaro
dc.contributor.referee1.fl_str_mv Iara Maria Carneiro de Camargo
dc.contributor.referee2.fl_str_mv Juliana de Carvalho Izidoro
dc.contributor.referee3.fl_str_mv Deovaldo de Moraes Júnior
dc.contributor.referee4.fl_str_mv Camilo Dias Seabra Pereira
dc.contributor.author.fl_str_mv Patricia Cunico Ferreira
contributor_str_mv Denise Alves Fungaro
Iara Maria Carneiro de Camargo
Juliana de Carvalho Izidoro
Deovaldo de Moraes Júnior
Camilo Dias Seabra Pereira
description Zeólitas sintetizadas a partir de cinzas leves e pesadas de carvão e modificadas com hexadeciltrimetilamônio (HDTMA) foram usadas como adsorvente para remoção dos corantes Solophenyl Navy (SN) e Solophenyl Turquesa (ST) e suas formas hidrolisadas, Solophenyl Navy hidrolisada (SNH) e Solophenyl Turquesa hidrolisada (STH), de efluente simulado de indústria têxtil. As zeólitas leve modificada (ZLM) e pesada modificada (ZPM) foram caracterizadas por diferentes técnicas, tais como, espectrometria de fluorescência de raios-X, difração de raios-X e microscopia eletrônica de varredura. As ZLM e ZPM apresentaram carga estrutural negativa devido à formação de uma bicamada parcial de HDTMA na superfície externa da zeólita. A concentração inicial dos corantes, o tempo de contato e o equilíbrio de adsorção foram avaliados. A cinética de adsorção de SN, ST, SNH e STH sobre as zeólitas seguiu o modelo de pseudo segunda- ordem. O tempo de equilíbrio foi de 20 min para SN e ST e 30 min para SNH e STH sobre ZLM, enquanto sobre ZPM foi de 60 min para SN e ST e 20 e 30 min para SNH e STH, respectivamente. Os modelos de Langmuir, Freundlich e Temkin foram aplicados para descrever as isotermas de adsorção. A adsorção dos corantes foi melhor descrita pelo modelo de Langmuir, com exceção dos sistemas SN/ZPM, SNH/ZPM e SNH/ZLM que seguiram modelo de Freundlich. As capacidades máximas de adsorção foram 3,64; 3,57; 2,91 e 4,93 mgL-1 para SN, ST, SNH e STH pela ZLM, respectivamente e 0,235; 0,492; 1,26 e 1,86 mgL-1 pela ZPM, nesta mesma ordem. O melhor desempenho dos corantes hidrolisados foi atribuído à redução do tamanho das moléculas dos corantes durante o processo de hidrólise. A toxicidade aguda dos corantes foi avaliada por diferentes organismos teste. O microcrustáceo C. dubia apresentou valores de EC50 de 1,25; 54,5; 0,78 e 2,56 mgL-1 para SN, ST, SNH e STH, respectivamente. A macrófita L. minor mostrou valores de EC50 de 18,9; 69,4; 10,9 e 70,9 mgL-1 para SN, ST, SNH e STH, respectivamente. As larvas de mosquitos C. tepperi mostraram valores de EC50 de 119 e 440 mgL-1 para a SN e ST, respectivamente. Com relação ao processo de adsorção, os efeitos agudos foram substancialmente reduzidos após o tratamento da solução aquosa de SN e ST com ZLM, assim como de suas formas hidrolisadas, apresentando nenhuma toxicidade após a remoção de 100% da cor. Após o tratamento dos corantes com ZPM houve um aumento da toxicidade, com exceção dos corantes SNH e STH que não apresentaram toxicidade após o tratamento. Testes de Avaliação e Identificação da Toxicidade foram realizados a fim de identificar quais substâncias estariam causando a toxicidade nos corantes SN, ST e no lixiviado de ZLM e ZPM. Os efeitos tóxicos foram reduzidos significativamente após a manipulação com Extração de Fase Sólida (SPE) e ácido etilenodiaminotetracético (EDTA) para o lixiviado de ZLM e ZPM. Os corantes mostraram redução na toxicidade após a manipulação com EDTA indicando que as substâncias tóxicas eram principalmente metais catiônicos.
publishDate 2015
dc.date.issued.fl_str_mv 2015-09-15
dc.type.status.fl_str_mv info:eu-repo/semantics/publishedVersion
dc.type.driver.fl_str_mv info:eu-repo/semantics/doctoralThesis
format doctoralThesis
status_str publishedVersion
dc.identifier.uri.fl_str_mv https://doi.org/10.11606/T.85.2015.tde-17112015-095220
url https://doi.org/10.11606/T.85.2015.tde-17112015-095220
dc.language.iso.fl_str_mv por
language por
dc.rights.driver.fl_str_mv info:eu-repo/semantics/openAccess
eu_rights_str_mv openAccess
dc.publisher.none.fl_str_mv Universidade de São Paulo
dc.publisher.program.fl_str_mv Tecnologia Nuclear
dc.publisher.initials.fl_str_mv USP
dc.publisher.country.fl_str_mv BR
publisher.none.fl_str_mv Universidade de São Paulo
dc.source.none.fl_str_mv reponame:Biblioteca Digital de Teses e Dissertações da USP
instname:Universidade de São Paulo (USP)
instacron:USP
instname_str Universidade de São Paulo (USP)
instacron_str USP
institution USP
reponame_str Biblioteca Digital de Teses e Dissertações da USP
collection Biblioteca Digital de Teses e Dissertações da USP
repository.name.fl_str_mv Biblioteca Digital de Teses e Dissertações da USP - Universidade de São Paulo (USP)
repository.mail.fl_str_mv virginia@if.usp.br|| atendimento@aguia.usp.br||virginia@if.usp.br
_version_ 1786376909230178304